Nikkelsoorten en chemische samenstelling
| Zuivere nikkelkwaliteit | Ni+Co | Cu | Si | Mn | C | Mg | S | Fe | Totaal onzuiverheden | UNS-aanduiding: |
| niet minder dan | ||||||||||
| N2 | 99.98 | 0.001 | 0.003 | .002 | .005 | .003 | .001 | .007 | .02 | |
| N4 | 99.9 | 0.015 | 0.03 | .002 | .01 | .01 | .001 | .04 | 0.1 | N02201 |
| N6 | 99.5 | 0.06 | 0.10 | .05 | .10 | .10 | .005 | .10 | 0.5 | N02200 |
| N8 | 99.0 | 0.15 | 0.15 | .20 | .20 | .10 | .015 | .30 | 1.0 | |
| DN | 99.35 | 0.06 | 0.02-0.10 | 0.05 | .02.10 | .02-.10 | .005 | .10 | 0.35 | |
| NY1 | 99.7 | 0.1 | 0.1 | - | .02 | .10 | .005 | .10 | 0.3 | |
| NY2 | 99.4 | 0.01-0.10 | 0.1 | - | - | - | 0.002-0.01 | .10 | 0.6 | |
| NY3 | 99.0 | 0.15 | 0.2 | - | 0.1 | 10 | 0.005 | .25 | 1.0 | |
| NMG0.1 | 99.6 | 0.05 | 0.02 | .05 | .05 | 0.07~0.15 | 0.005 | .07 | .40 | |
| NSI0.19 | 99.4 | 0.05 | 0.15~0.25 | .05 | .10 | .05 | 0.005 | .07 | .50 | |
De corrosieweerstand van nikkel
Nikkel is bijzonder bestand tegen alkalicorrosie en is relatief stabiel in alkali op hoge temperatuur of in vlamsmelten, dus het wordt voornamelijk gebruikt in de alkali-industrie. Bij normale temperatuur is de slak extreem stabiel in zeewater, zoutoplossing en organisch medium (zoals vetzuur, fenol, fermentatie, enz.), En is niet bestand tegen anorganische zuurcorrosie, noch stabiel in azijnzuur en licht zuur.